Abstract |
This study investigated time to first failure of stainless steel orthodontic first permanent molar tubes (Ormco Corp) bonded with a light-cured resin adhesive ( Transbond) and assessed whether this was related to patient gender, age of the patient at the start of treatment, the presenting malocclusion, or the operator. All first molar tubes were bonded to intact buccal enamel, free of any restoration. Survival analysis was carried out on data from 483 patients with 1190 bonded first molar tubes. For each case, a single molar tube, either that which was first to fail or had the shortest follow-up time, was chosen for analysis. The median time until first bonded tube failure was 699 days with an overall failure rate of 21% recorded. There was no significant difference in time to first failure of molar tubes with respect to patient gender or presenting malocclusion but significant differences were recorded with respect to the patients' age at the start of treatment and the operator. Age at the start of treatment and operator were identified as independently useful predictors of bonded molar tube survival.
|
Authors | D T Millett, A Hallgren, A C Fornell, M Robertson |
Journal | American journal of orthodontics and dentofacial orthopedics : official publication of the American Association of Orthodontists, its constituent societies, and the American Board of Orthodontics
(Am J Orthod Dentofacial Orthop)
Vol. 115
Issue 6
Pg. 667-74
(Jun 1999)
ISSN: 0889-5406 [Print] United States |
PMID | 10358250
(Publication Type: Journal Article)
|
Chemical References |
- Stainless Steel
- Transbond
- Bisphenol A-Glycidyl Methacrylate
|
Topics |
- Adolescent
- Adult
- Age Factors
- Bisphenol A-Glycidyl Methacrylate
- Child
- Child, Preschool
- Clinical Competence
- Dental Bonding
- Equipment Failure
- Equipment Failure Analysis
- Female
- Humans
- Male
- Malocclusion
(classification)
- Molar
- Orthodontic Brackets
- Orthodontic Wires
- Proportional Hazards Models
- Retrospective Studies
- Risk Factors
- Sex Factors
- Stainless Steel
- Survival Analysis
|